that is some heat rejection for the 31% vlt callled 30% it rejects 61% that will compete with huper in my town even most 35% metallized films only reject 40-45%

Link to comment

FILM TYPE COLOR IR

REJECTION VISIBLE LIGHT TRANSMISSION SOLAR ENERGY

REJECTED SHADING

COEFFICIENT SOLAR HEAT GAIN

COEFFICIENT VISIBLE LIGHT REFLECTION SOLAR ENERGY ABSORBED GLARE REDUCTION

IR 70 neutral 47% 71% 32% 0.78 0.68 10% 32% 25%

IR 60 neutral 60% 60% 41% 0.68 0.59 11% 43% 37%

IR 50 neutral 70% 50% 49% 0.60 0.52 12% 51% 47%

IR 40 neutral 76% 42% 54% 0.54 0.46 14% 54% 56%

IR 30 neutral 85% 31% 61% 0.46 0.40 17% 61% 67%

Link to comment

I'm looking forward to working with this film, although I think most people will like it better when they come out with a less reflective version.

They say it's made with Titanium Nitride which is the stuff often used on the gold colored drill bits you see that are "Titanium Coated" :thumb