In cooperation with NATO ISAF and VAT we did some tests. Of course they were quite different from famous lab tests, but as our soldiesr going to Afganistan soon, we don't think that lab rats advices and test reports will be helpfull and usefull. Here I will post some pictures and later I will make video.

I don't know the name of this NATO grenade exploded under the glass, but it was loud :rollin

DSC_9477.jpg

DSC_9469.jpg

Link to comment
Share on other sites

As a result of tests we saw that regular car glass with films installed from both sides will help soldiers to survivae in case near explosion of hand grenade and other explosives.....Also we did some ballistic tests. Results was not so nice - but we were waiting it. As M16 which we used and also GLOCK are strong weapons. Also for our films :rollin:rollin:beer

DSC_9502.jpg

DSC_9492.jpg

DSC_9491.jpg

Link to comment
Share on other sites

How thick is the installed film? How was the film anchored (batten or wet seal, or other?) Exterior/interior application. .both?

Is there a specific standard there? Type of glass? Thickness? . .just curious if the NATO standard is different than DoD standards here in USA?

Thx

Link to comment
Share on other sites

That's not an M16, that's an H&K G3. It fires a 7.62 (.308 win) instead of the 5.56 like an M16.

Don't sell yourself short, it got shot by a bigger bullet!

Ahaaaaaaaaaaaaa, thanks Sir! I am not specialist in Your (now ours :barf ) weapons.

Guys told us that will be M16 - 7,62 and other one with 5,56 bullet.

I C. Anycase it passed through - and I have no idea it will work.

Here U can see moment whe ONE bullet from GLOCK were stopped - this moment is pictured

DSC_9522.jpg

DSC_9521.jpg

But as we did grenade tests - which we passed, we decide also to shoot.

Link to comment
Share on other sites

How thick is the installed film? How was the film anchored (batten or wet seal, or other?) Exterior/interior application. .both?

Is there a specific standard there? Type of glass? Thickness? . .just curious if the NATO standard is different than DoD standards here in USA?

Thx

There were 2 films on each glass.

8 mil - 6 mm regular (not tempered) glass - 21 mil window film

8 mil - 6 mm regular (not tempered) glass - 16 mil window film

It was anchired with piece of metall - I will try to find pictured, deepnes of anching around one inch.

We tested using our ideas and methods. The situation is that standarts are invented by smart heads in labs. These guys will go to Afganistan shortly. We make tests with organization XX Century Wars Veterans Against Terror (VAT) - mainly there are veterans of previous afgan war. As latvian HUMMERS were exploded in Iraq some month ago, we look how can work glass if grenade will explode near, and if it can help to avoid any problems in case instaled on a car. That was our aim. Same tests was done at Camp Marmal military base by German bundeswer forces.....No any standarts "fallen ballZ" :barf - just REAL LIFE TESTS.

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

  •   Sponsored by
    auto-precut.com

    signwarehouse

    martinmetalwork.com

    tinttek

    filmvinyldesigns

    ride wrap

    Conco

    Lexen

    tintwiz

  • Activity Stream

    1. 7

      Air80 vs Stratos70 Windshield

    2. 7

      Air80 vs Stratos70 Windshield

    3. 0

      Process

    4. 7

      Air80 vs Stratos70 Windshield

    5. 0

      PPF installer for hire in SoCAL

    6. 11

      Boat window tinting tips

    7. 11

      Boat window tinting tips

×
×
  • Create New...